啊灬啊灬啊灬快灬高潮了,99久久亚洲精品无码毛片,中文字幕无码日韩专区免费,成人H视频在线观看

銷售咨詢熱線
15953126901
18615254757
行業動態 dongnews
企業案例 case

聯系我們

  • 聯系人:濟南燕翔鐵藝制品有限公司
  • 手機:15953126901
  • 電話:18615254757
  • 郵箱:785385551@qq.com
  • 地址:濟南市天橋區歷山北路黃臺不銹鋼市場3區317
當前位置: 首頁 > 新聞資訊>行業動態 鐵藝護欄的防銹處理方式

鐵藝護欄的防銹處理方式

來源:http://www.lpylmy.com 日期:2021-11-15 發布人: 瀏覽次數:23
1.酸洗前檢查處理
1. Inspection and treatment before pickling
檢查鐵藝工件是否具備本廠鍍鋅的工藝孔(排氣、出入鋅夜、吊掛),鐵藝工件表面的銹蝕程度,表面覆蓋物能否被鹽酸除去(如有油漆、油脂等應采用火燒、打磨、堿洗等法除去)。
Check whether the iron work piece has the galvanized process hole of the factory (exhaust, zinc in and out, hanging), the degree of corrosion on the surface of the iron work piece, and whether the surface covering can be removed by hydrochloric acid (if there is paint, grease, etc., it shall be removed by fire, grinding, alkali washing, etc.).
2.脫脂(堿洗)
2. Degreasing (alkali washing)
配有加熱設備,消除鐵藝工件表面的油脂、涂料等。
Equipped with heating equipment to eliminate grease, coating, etc. on the surface of iron workpieces.
3.水洗
3. Water washing
清除鐵藝工件表面的堿水及附著物。
Remove alkali water and attachments on the surface of wrought iron workpieces.
4.酸洗
4. Pickling
除去鐵銹、氧化皮等其它表面覆蓋物。
Remove rust, scale and other surface coverings.
5.酸洗后檢查處理:
5. Inspection and treatment after pickling:
酸洗效果是否理想,如酸洗不充分,再次酸洗,如果酸洗前處理不徹底,需重新處理后再次酸洗。
Whether the pickling effect is ideal. If the pickling is insufficient, pickling shall be carried out again. If the treatment before pickling is not complete, pickling shall be carried out again after re treatment.
濟南鐵藝護欄
6.水洗
6. Water washing
除去鐵藝工件表面的酸水及其它附著物。
Remove acid water and other attachments on the surface of iron work pieces.
7.上助鍍劑
7. Plating aid
再次清洗工件表面,保證表面在鍍鋅之前不在生銹。
Clean the workpiece surface again to ensure that the surface does not rust before galvanizing.
8.烘干
8. Drying
提高鐵藝工件溫度,避免鐵藝表面水分過多,在鍍鋅時發生爆炸。
Raise the temperature of wrought iron workpiece to avoid excessive moisture on the surface of wrought iron and explosion during galvanizing.
9.熱浸鋅
9. Hot dip galvanizing
工件浸泡于440℃-470℃熔融的鋅液中,達到一定時間后提出,鐵藝工件表面被獲得一層鋅鐵合金層和純鋅層鍍層。
After the workpiece is immersed in molten zinc at 440 ℃ - 470 ℃ for a certain time, a layer of zinc iron alloy layer and pure zinc layer are obtained on the surface of iron workpiece.
10.鈍化
10. Passivation
提供工件表面抗大氣的腐蝕性能,減少或延長白銹出現的時間。
Provide atmospheric corrosion resistance of workpiece surface to reduce or prolong the time of white rust.
11.冷卻
11. Cooling
防止工件激冷回縮,產生集體組織開裂。
Prevent the workpiece from chilling and retracting, resulting in collective structure cracking.
12.檢驗
12. Inspection
鍍層的檢驗和測定,工件的外觀檢查。
Inspection and measurement of coating and appearance inspection of workpiece.